Sign In | Join Free | My chinaqualitylighting.com
chinaqualitylighting.com
Products
Search by Category
Wholesale Marketplace
Home > Machine Tools Accessory >

ISO Shrinkage Injection Moulding Solutions OEM

Categories Injection Molding Solution
MOQ: 100pcs
Price: Negotiable
Payment Terms: T/T
Supply Ability: More than 1 million
Delivery Time: 30day
Packaging Details: As the customer required
Place of Origin: CHINA
Brand Name: OEM
Certification: ISO
Emphasize: Reprint Books In A Reduced Format Cause And Countermeasure Analysis
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

ISO Shrinkage Injection Moulding Solutions OEM

The Cause And Countermeasure Analysis Of Shrinkage In Products

Reprint Books In A Reduced Format

Shrinkage refers to the depression of the product table and the production of insects, like hair in the thicker part of the wall. In the process of cooling the molten resin from the external part, when the volume shrinkage cannot be compensated, the resin on the surface of the formed product is subjected to the volume shrinkage of the molten resin in 6 parts, resulting in the formation of q marks.

CauseCuntermeasure
Forming condition

1. There are many cases of insufficient pressure and retaining pressure during the injection period

2. The pressure retention time is insufficient

4. The mold temperature is not appropriate, the mold temperature is too low, the gate curing fast, pressure retention failure is easy to produce shrinkage hole: the mold temperature is too high, setting the appropriate mold temperature is easy to produce shrinkage marks

5. The injection speed is too fast

The temperature of the material is too high, and the shrinkage of the material is too large

1. Increase the injection pressure and pressure holding pressure; 2. Increase the pressure raising time

3. Increase the measurement distance

4. In thick products, this tendency is stronger and the speed is reduced

5. Properly reduce the temperature of the material


Die

1. The runner and gate are too small. 2. Improper placement of pouring II makes the material flow distance too long

3. Insufficient or inconsistent mold cooling


1. Increase the section of runner and gate

2. Review runner and gate

3. Check the cooling system


Product Design

1. Uneven thickness

2. The shape of tendons is not standard


1. Avoid uneven thickness, can use stolen thick pin or groove.

2. Avoid thick and long tendons

Material

1. The shrinkage rate of materials is too large

2. Poor material fluidity


1. Switch to materials with low shrinkage

2. Improve material mobility

OtherScrew check ring is damagedReplace the check ring

Buy ISO Shrinkage Injection Moulding Solutions OEM at wholesale prices
Send your message to this supplier
 
*From:
*To: Sun On Plastic Moulding Limited
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0