Brand Name:Zhiyou Model Number:AWS E2209-16 Place of Origin:Shanghai China Austenitic Ferritic Stainless Steel AWS Welding Electrode Material E2209-16 Application: E2209-16 is for welding extra-low carbon stainless steel structures in petrochemical and hydraulic projects industries,e.g.structures fabricated by 00Cr22Ni5NiMo3N ... |
Shanghai Zhiyou Marine & Offshore Equipment Co.,Ltd.
Shanghai |
![]() |
Place of Origin:China Mainland Brand Name:Product's brand provided at your need. Model Number:There is no specific model. The production of all products is processed according to the CAD drawings provided by customers. ...Welding Aluminum Welding Procedures CNC Machining MIG welding aluminum TIG Metal Welding We are a professional factory specializing in aluminum hardware processing. Our comprehensive processing services cover a wide range of techniques, including CNC machining, welding... |
Zhongshan Shanfeng CNC Welding Aluminum Products Co., Ltd.
Guangdong |
![]() |
Brand Name:Hongfa Model Number:HF007 Place of Origin:Guangdong China ... 3 Single span, double-span, multi-span 4 single floor, double floors...... 5 Column Q235, Q345 / S275/ S355 welded H section steel/ Box Section/ Trusse Section 6 Beam Q235, Q345 / S275/ |
Hongfa Steel Structure Mats. Co., Ltd.
Guangdong |
![]() |
Brand Name:HUATEC Model Number:Fillet Weld Cam Type Weld Gauge Place of Origin:Beijing ...AWS Gage Welding Seam Gauge Cam type weld gauge,single purpose welding gage, internal Hi- Lo gage,rootweld spacing gauge,measure interrior misalignment, measure fillet weld size etc. Welding inspection gauge is a test weld appearance quality of the most simple and effective method, its content is carried out on the weld... |
HUATEC GROUP CORPORATION
Beijing |
![]() |
Brand Name:Victory Model Number:Ernicrmo-4 Place of Origin:China Product Description: Nickel Welding Wire ERNiCrMo-4 welding wire is a high-performance welding material widely used in the chemical industry. It is composed of elements such as nickel, chromium, molybdenum and iron. It has excellent corrosion resistance... |
Changzhou Victory Technology Co., Ltd
Jiangsu |
![]() |
Brand Name:Dehai Boiler Model Number:Superheater Place of Origin:China Good quality Industry Boiler Pressure and Superheater Tubes EN 3834 Welding procedure Description of Superheaters 1. Whatever type of boiler is used, steam will leave the water at its surface and pass into the steam space. Steam formed above the water ... |
Zhangjiagang Dehai Boiler Co., Ltd
|
![]() |
Brand Name:Highlight Model Number:HT-033 Place of Origin:China MOBILE TELECOM TOWER MICROWAVE TOWER ASTM A36 ASTM A572 First of all, we have our own hot dip galvanzation plant! All towers must via trial assembly and 8 items in house inspection with report! 1. Design code: 1) Major standard: ANSI/TIA‐222‐F/G 2). ... |
Highlight Steel tower Co.,Ltd.
|
![]() |
Brand Name:LONGTENG Model Number:LT·H10Mn2 Place of Origin:CHINA ...Aws A5.17 Eh14 Submerged Arc Saw Welding Wire 2.5mm 3.2mm 4.0mm 5.0mm LT·H10Mn2 2.5/3.2/4.0/5.0mm Submerged Arc Welding Wire AWS A5.17 EH14 Submerged arc welding wire is a copper coated steel wire, and it can be used in automatic submerged arc welding with welding flux. The weld metal has excellent mechanical properties. LT·H10Mn2 Conform to Standard :GB/T 5293 H10Mn2 AWS... |
Longteng Special Steel Group
Jiangsu |
![]() |
Brand Name:XL-TITANIUM Place of Origin:China AWS A5.16 Ti6AL4V Titanium Alloy Welding Wires Products Introduction Titanium welding wires are made as filler metal for welding applications by arc, MIG, TIG procedures. Titanium welding wires we supply can only be round cross section and made from ... |
Baoji Xinlian Titanium Industry Co.,Ltd.
Shaanxi |
![]() |
Brand Name:Changsheng Model Number:AWS A5.16 Place of Origin:China ... and anodizing, where parts are hung or tied down with wire. “Ti” Wire- AWS A5.16 Titanium ERTi-7 Welding Wire for TIG welding is cut to 36″ lengths and is also available in common welding rod sizes. Specification of our AWS A5.16 Titanium ERTi-7 |
Baoji City Changsheng Titanium Co.,Ltd
|
![]() |
Brand Name:DLX Model Number:ErNiFe-6 Place of Origin:China Jiangsu AWS A5.14 1.6mm ErNiFe-6 incoloy alloy filling wire from manufacturer Nickel Based Welding Wire Nickel based welding wire ERNiCrFe-6 is a nickel-based filler metal for welding. Changzhou DLX alloy is one of the main producer in China for the ErNiCrFe-6 welding wire. ErNiCrFe properties are appropriate for the as-welded condition. Also ERNiCrFe-6 is the AWS... |
Changzhou DLX Alloy Co., Ltd.
Jiangsu |
![]() |
Brand Name:OSLAND Place of Origin:China Model Number:AWS ER5356 AWS ER4043 ... rod, low silicon welding rod, high silicon welding rod.The aluminum welding wires are widely used in bicycles, aluminium scoter, engine carriage, pressure vessel, armary processing, ship-building, space shuttle etc. Application: Aluminum welding wire is a |
Osland Metals Limited
Hebei |
![]() |
Place of Origin:China Brand Name:SOE Model Number:ENiFe-C1 (Z408) ...AWS ENi-C1: Repair welding of various kinds of cast iron products. Deposits nearly pure nickel which is easy machinable AWS ENiFe-C1 : Repair welding of important great cast iron and nodular cast iron AWS ENiCu-B : Repair welding of grey cast iron strength of which is not so highly required 2..Chemical Composition (%) Product C Si Mn S Ni Fe Cu/ Other GB AWS... |
Shanghai Overseas Enterprises Co., Ltd.
Shanghai |
![]() |
Brand Name:Eternal Bliss Model Number:EB2912 Place of Origin:China ... and gear bronze ,hard-surfacing of axle bush. Applications: AWS ECuSn-C copper brazing alloy welding electrode is applied in welding of similar and dissimilar metal,such as copper,brass and gear bronze,hard-surfacing of axle vanes of ships,hard facing or |
Eternal Bliss Alloy Casting & Forging Co.,LTD.
Jiangsu |
![]() |
Brand Name:CHENXIANG Model Number:H08A/AWS EL8 Place of Origin:Shandong, China ...AWS EL8 H08A 4.0mm 5.0mm Submerged Arc Welding Wire Product Description H08A submerged arc welding wire is a commonly used carbon steel welding wire, mainly used in submerged arc welding (SAW) process. It is usually used with flux and is suitable for welding low carbon steel and low alloy steel. H08A welding wire has low carbon content and low impurity content, and the welded... |
Hainan Chenxiang New Material Technology Co., Ltd.
Shandong |
![]() |
Brand Name:WUXI SYLAITH Model Number:C11000 C10200 C12000 C12200 Place of Origin:Jiangsu China (Mainland) ...Welding Wire AWS A5.18 ER70S-6 Gas Shielded Mig Welding Wire AWS A5.18 ER70S-6 Standard: GB/T ER50-6/ DIN SG2/ JIS YGW12 AWS ER70S-6/ BS A18/ EN G3Si1 Gas Shielded Mig Welding Wire AWS A5.18 ER70S-6 Description: Welding Wire ER70S-6 (SG2) is a copper coated low alloy steel wire shielded by 100% CO2 with all position welding. The wire has a very good welding... |
WUXI SYLAITH SPECIAL STEEL CO.,LTD
Jiangsu |
![]() |
Brand Name:TMTeck Place of Origin:China ...AWS) Resolution Calibration Block Specifications: AWS D1.1/D1.1M-2015 Calibration Functions: Angle Beam: resolution (45°, 60°, 70°). Also called an RC block, the AWS Resolution Reference Block is used for checking resolution capabilities of angle beam transducers. Contains three sets of 0.0625" diameter through-holes for 45°, 60° and 70°. In accordance with AWS Welding Highway and Railway Bridges specification D2.0, and Structural Welding |
TMTeck Instrument Co., Ltd
Beijing |
![]() |
Brand Name:LHTI Model Number:Titanium welding wire Place of Origin:Baoji ,Shaanxi ,China AWS B863 aws a 5.16 0.8mm 1.0mm 1.2mm titanium wire straight rod for welding Titanium welding wire has excellent welding process performance, beautiful weld formation, and its welded metals have excellent comprehensive mechanical properties. Mainly used for welding of titanium-based alloys. Radiographic inspection requirements for weld... |
Baoji Lihua Nonferrous Metals Co., Ltd.
Shaanxi |